AMS 7725E class3 tungsten alloy bar has better machinability, very good mechanical properties, and high absorption capacity for X-rays and gamma rays. It can be applied in the radiation shielding material and radiation-protective equipment.
The properties of AMS 7725E class3 tungsten alloy bar are:
Matrix: 95% W
Density: 17.75~17.35g/cc
Hardness Rockwell Max: 34HRC
AMS 7725E: Class3 Type1
Ultimate Tensile Strength: 94 KSI and 648 MPa
Yield Strength (0.2% offset): 75 KSI and 517 MPa
Elongation: 1%
AMS 7725E: Class3 Type2
Ultimate Tensile Strength: 105 KSI and 724 MPa
Yield Strength (0.2% offset): 75 KSI and 517 MPa
Elongation: 3%