HPM1701 tungsten alloy rod has high density and is machinable. Its ingredient is 90% tungsten、10% nickel and copper. It is intended for uses such as weights or counter-balances in static or dynamic balancing, high-speed rotating inertia members, radiation shielding, hypervelocity impact, and vibration-damping applications.
The properties of WA1895 tungsten alloy rod are:
Matrix: 90% W
Binder: 10% Ni-Cu
Density: 17.0g/cm3 and 0.614lb/in3
Thermal Conductivity: 95 W/(m?K)
Coefficient of Thermal Expansion 20~100℃:6.0μm/(m?K)
Coefficient of Thermal Expansion 20~300℃:6.2μm/(m?K)
Coefficient of Thermal Expansion 20~4500℃:6.4μm/(m?K)
Electrical Conductivity: 14% IACS
Electrical Resist:0.12~0.13μΩ?m
Yield Strength (0.2% offset): 75.4~79.8KSI
Tensile Strength: 94.3~110 KSI
Elongation: 1~4%
Hardness:270~310HV10
Modulus of Elasticity:280~340GPa
Magnetic Properties: Non-magnetic
More details, please visit:
http://www.tungsten-alloy.com/tungsten-alloy-rod.html